Vacuum Induction Melting K418b Superalloy Block for Industrial Turbine
Click to enlarge

Vacuum Induction Melting K418b Superalloy Block for Industrial Turbine

China ZhejiangZhejiang Zegota Precision Technology Co., Ltd.

US$69.90

MOQ1000 Pieces

Product profile

Surface
Bright
Density
8.0g/cm3
Heat Conductivity
10.15 λ/(W(M ºC)
Length
as Request

Company profile

Zhejiang Zegota Precision Technology Co., Ltd.

浙江泽广泰精密科技有限公司
China ZhejiangRoom 703, Building 11, Intelligent Industry Innovation Park, Jiaxing Economic Development Zone, Jiaxing, Zhejiang, China
  • CertifiedVerified Supplier
  • Business Type: Trading Company
  • Established: 2018
  • Employees: 5
  • Plant Area: 245.0m²
  • Avg. Response Time: ≤ 1.51h
  • Certification: -

Main Products

  • Biochips
  • Glass Vials
  • Chitosan
  • Profiled/Shaped Wire
  • Clad Wire
  • Feeder
  • 3D Printing Services
  • Medical Supplies
  • Dressing
  • Rubber Stopper

Main Markets

South America,East Asia(Japan/ South Korea),Australia,North America